Skip to Main Content
ASM Handbook

Powder Metallurgy

Edited by
P. Samal
P. Samal
Search for other works by this author on:
J. Newkirk
J. Newkirk
Search for other works by this author on:
ASM International
Volume
7
ISBN electronic:
978-1-62708-175-7
Publication date:
2015
Book Chapter

Bulk Properties of Powders[1]

By
Sydney H. Luk
Sydney H. Luk
Revising author
Höganäs AB
Search for other works by this author on:
Published:
2015
Page range:
111 - 126
Publication history
August 20, 2015

Abstract

This article describes the methods for determining the flow rate of metal powders. It examines the factors affecting flow rate, apparent density, and angle of repose of metal powders. The article reviews the frictional properties, cohesive strength, tap density, and compressibility of metal powders. It explains the mechanisms of powder segregation. The article provides information on green strength and springback value of rectangular test bar. It concludes with a discussion on the chemical composition of metal powders.

You do not currently have access to this content.
Don't already have an account? Register

Sydney H. Luk, 2015. "Bulk Properties of Powders", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal