Skip to Main Content
ASM Handbook

Powder Metallurgy

Edited by
P. Samal
P. Samal
Search for other works by this author on:
J. Newkirk
J. Newkirk
Search for other works by this author on:
ASM International
Volume
7
ISBN electronic:
978-1-62708-175-7
Publication date:
2015
Book Chapter

Compaction of Carbide Powders

By
Neal Myers
Neal Myers
Kennametal Inc.
Search for other works by this author on:
Pankaj K. Mehrotra
Pankaj K. Mehrotra
Kennametal Inc.
Search for other works by this author on:
Published:
2015
Page range:
715 - 719
Publication history
August 26, 2015

Abstract

Consolidation and shaping of grade powders is carried out using several methods, depending on the size, complexity, shape, and quantity of parts required. This article details the powder consolidation methods of carbide powders: uniaxial pressing, cold isostatic pressing, extrusion, green machining, and injection molding.

You do not currently have access to this content.
Don't already have an account? Register

Neal Myers, Pankaj K. Mehrotra, 2015. "Compaction of Carbide Powders", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal