Pressing and Sintering of Titanium Powders

By
Vladimir Duz
Vladimir Duz
ADMA Products, Inc.
Search for other works by this author on:
Vladimir Moxson
Vladimir Moxson
ADMA Products, Inc.
Search for other works by this author on:
Mykhailo Matviychuk
Mykhailo Matviychuk
ADMA Products, Inc.
Search for other works by this author on:
M. Ashraf Imam
M. Ashraf Imam
The George Washington University, Department of Mechanical and Aerospace Engineering
Search for other works by this author on:
Published:
2015
Page range:
650 - 659
Publication history
August 27, 2015

Abstract

Consolidation of titanium powders at room temperature may be performed by low-cost conventional powder metallurgy processes. This article provides information on various consolidation methods, namely, die pressing, direct powder rolling, and cold isostatic pressing. It also describes the sintering of blended elemental powders, high-strength titanium alloys, and porous material as well as the sintering of titanium powders by microwave heating.

You do not currently have access to this content.
Don't already have an account? Register

Vladimir Duz, Vladimir Moxson, Mykhailo Matviychuk, M. Ashraf Imam, 2015. "Pressing and Sintering of Titanium Powders", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal