Surface Area, Density, and Porosity of Powders

By
Sydney Luk
Sydney Luk
Revising author
Höganäs AB
Search for other works by this author on:
Published:
2015
Page range:
132 - 144
Publication history
December 18, 2015

Abstract

This article focuses on the theory, advantages, and limitations of various methods used for the determination of surface area, density, and porosity of powder. These include gas adsorption, permeametry, pycnometry, and mercury porosimetry. Information on various equipment used in these processes are also provided.

You do not currently have access to this content.
Don't already have an account? Register

Sydney Luk, 2015. "Surface Area, Density, and Porosity of Powders", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal