Skip to Main Content
ASM Handbook

Powder Metallurgy

Edited by
P. Samal
P. Samal
Search for other works by this author on:
J. Newkirk
J. Newkirk
Search for other works by this author on:
ASM International
Volume
7
ISBN electronic:
978-1-62708-175-7
Publication date:
2015
Book Chapter

Metal and Alloy Powders for Welding, Hardfacing, Brazing, and Soldering[1]

By
Bo Hu
Bo Hu
Revising author
North American Höganäs, Inc.
Search for other works by this author on:
Published:
2015
Page range:
769 - 782
Publication history
August 29, 2015

Abstract

Metals and alloy powders are used in welding, hardfacing, brazing, and soldering applications, which include hardface coatings, the manufacturing of welding stick electrodes and flux-cored wires, and additives in brazing pastes or creams. This article reviews these applications and the specific powder properties and characteristics they require.

You do not currently have access to this content.
Don't already have an account? Register

Bo Hu, 2015. "Metal and Alloy Powders for Welding, Hardfacing, Brazing, and Soldering", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal