Ferrous Powder Metallurgy Metallography[1]

By
Thomas F. Murphy
Thomas F. Murphy
Hoeganaes Corp.
Search for other works by this author on:
Published:
2015
Page range:
156 - 167
Publication history
August 18, 2015

Abstract

Metallographic analysis is primarily a collection of visual and imaging techniques that provide an insight into the background of a material or part and its behavior. Metallic specimens, both porous and pore-free, are opaque, and as a result, an optical examination must be performed on carefully prepared planar (two-dimensional) surfaces. This article discusses the preparation sequence of ferrous powders, which is normally separated into several well-defined steps: sample selection, sectioning, mounting, grinding, polishing, drying, and chemical etching and/or coating. It provides several suggestions to promote and encourage the safety of those performing metallographic preparation and analysis.

You do not currently have access to this content.
Don't already have an account? Register

Thomas F. Murphy, 2015. "Ferrous Powder Metallurgy Metallography", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal