Powder Metallurgy Stainless Steels Applications

By
Prasan K. Samal
Prasan K. Samal
Consultant
Search for other works by this author on:
Roland Warzel, III
Roland Warzel, III
North American Höganäs
Search for other works by this author on:
Suresh O. Shah
Suresh O. Shah
Cloyes Gear and Products Inc.
Search for other works by this author on:
Published:
2015
Page range:
480 - 487
Publication history
August 24, 2015

Abstract

This article describes the physical properties of powder metallurgy (PM) stainless steels. These include thermal diffusivity, conductivity, thermal expansion coefficient, Poisson's ratio, and elastic modulus. The article contains a table that lists the characteristics of various grades of PM stainless steels. It discusses the applications of various PM stainless steels such as rearview mirror brackets, anti-lock brake system sensor rings, and automotive exhaust flanges and sensor bosses.

You do not currently have access to this content.
Don't already have an account? Register

Prasan K. Samal, Roland Warzel, III, Suresh O. Shah, 2015. "Powder Metallurgy Stainless Steels Applications", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal