Specialty Applications of Metal Powders

By
Jack A. Hamill, Jr.
Jack A. Hamill, Jr.
Reviewing author
Hoeganaes Corporation
Search for other works by this author on:
Published:
2015
Page range:
20 - 30
Publication history
August 17, 2015

Abstract

Metal powders are used as fuels in solid propellants, fillers in various materials, such as polymers or other binder systems, and for material substitution. They are also used in food enrichment, environmental remediation market, and magnetic, electrical, and medical application areas. This article reviews some of the diverse and emerging applications of ferrous and nonferrous powders. It also discusses the functions of copier powders and the processes used frequently for copier powder coating.

You do not currently have access to this content.
Don't already have an account? Register

Jack A. Hamill, Jr., 2015. "Specialty Applications of Metal Powders", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal