Skip to Main Content
ASM Handbook

Powder Metallurgy

Edited by
P. Samal
P. Samal
Search for other works by this author on:
J. Newkirk
J. Newkirk
Search for other works by this author on:
ASM International
Volume
7
ISBN electronic:
978-1-62708-175-7
Publication date:
2015
Book Chapter

History of Powder Metallurgy

By
James P. Adams
James P. Adams
Revising author
MPIF and APMI International
Search for other works by this author on:
Published:
2015
Page range:
3 - 8
Publication history
August 17, 2015

Abstract

Powder metallurgy (PM) has been called a lost art. Long before furnaces were developed that could approach the melting point of metal, PM principles were used. This article provides an overview of the major historical developments of various methods of platinum powder production. The development of production methods took place in various phases starting from prehistoric time, post-war period, to recent and commercial period. The article discusses the powder metallurgy of platinum, as well as the commercial and post-war developments of PM. Literature and trade associations are also discussed.

You do not currently have access to this content.
Don't already have an account? Register

James P. Adams, 2015. "History of Powder Metallurgy", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal