Abstract

This article focuses on mechanical testing characterization of blended elemental powder metallurgy (PM) titanium alloys and prealloyed PM titanium alloys. It examines the tensile properties, fracture toughness, stress-corrosion threshold resistance, fatigue strength, crack propagation properties, and processing-microstructure-property relationships of these alloys. The article also reviews five considerations for powder process selection.

Abstract

This article provides a summary of the conventional technologies used for titanium powder production. It focuses on the various processes for titanium powder production, namely, Hunter, Kroll, Armstrong, MER, TIRO, FFC-Cambridge, Chinuka, and CSIR processes. Employment of titanium powder significantly improves the synthesis of titanium and its alloys.

You do not currently have access to this content.
Don't already have an account? Register

2015. "Powder Metallurgy Titanium and Titanium Alloys", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal