Powder Metallurgy Carbon and Low-Alloy Steels

Published:
2015

Abstract

This article summarizes the general classification, mechanical properties, and applications of ferrous powder metallurgy (PM) materials for parts production. It discusses four principal ferrous PM alloy types: admixed elemental alloys, diffusion alloys, prealloys, and hybrid alloys. The article reviews the benefits and disadvantages as well as the effect of processing on the properties and material microstructure of these alloys. It contains tables that list the mechanical properties of various iron-copper and copper steels.

Abstract

This article briefly reviews the production methods and characteristics of plain carbon and low-alloy water-atomized iron and steel powders, high-porosity iron powder, carbonyl iron powder, and electrolytic iron powder. It emphasizes on atomized powders, because they are the most widely used materials for ferrous powder metallurgy. The article provides information on the properties and applications of these powders. It also includes an overview of diffusion alloying, basics of admixing, and bonded premixes.

You do not currently have access to this content.
Don't already have an account? Register

2015. "Powder Metallurgy Carbon and Low-Alloy Steels", Powder Metallurgy, P. Samal, J. Newkirk

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal