Skip to Main Content
ASM Handbook

Surface Engineering

Edited by
C.M. Cotell
C.M. Cotell
Search for other works by this author on:
J.A. Sprague
J.A. Sprague
Search for other works by this author on:
F.A. Smidt, Jr.
F.A. Smidt, Jr.
Search for other works by this author on:
ASM International
Volume
5
ISBN electronic:
978-1-62708-170-2
Publication date:
1994
Book Chapter

Ceramic Coatings and Linings

By
Woodrow W. Carpenter
Woodrow W. Carpenter
Revising author
The Ceramic Coating Company
Search for other works by this author on:
Published:
1994
Page range:
469 - 481

Abstract

Ceramic coatings are applied to metals to protect them against oxidation and corrosion at room temperature and at elevated temperatures. This article provides a detailed account of the factors to be considered when selecting a ceramic coating and describes the characteristics of various coating materials, namely, silicate glasses, oxides, carbides, silicides, and cermets. It reviews ceramic coating methods: brushing, spraying, dipping, flow coating, combustion flame spraying, plasma-arc flame spraying, detonation gun spraying, pack cementation, fluidized-bed deposition, vapor streaming, troweling, and electrophoresis. The article also includes information on the evaluation of the quality of ceramic coatings.

You do not currently have access to this content.
Don't already have an account? Register

Woodrow W. Carpenter, 1994. "Ceramic Coatings and Linings", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal