Skip to Main Content
ASM Handbook

Surface Engineering

Edited by
C.M. Cotell
C.M. Cotell
Search for other works by this author on:
J.A. Sprague
J.A. Sprague
Search for other works by this author on:
F.A. Smidt, Jr.
F.A. Smidt, Jr.
Search for other works by this author on:
ASM International
Volume
5
ISBN electronic:
978-1-62708-170-2
Publication date:
1994
Book Chapter

Classification and Selection of Finishing Processes

By
K. Subramanian
K. Subramanian
World Grinding Technology Center, Norton Company
Search for other works by this author on:
Published:
1994
Page range:
81 - 83

Abstract

This article focuses on the various technology drivers for finishing methods, namely, tolerance, consistency, surface quality, and productivity. Every finishing method may be viewed as a manufacturing system consisting of four input categories: machine tool, processing tool, work material, and operational factors. The article provides a classification of finishing as a surface generation process and addresses the characteristics of the generated surfaces and the methods used to measure them. It describes the thermomechanical interactions occurring between the processing tool and the work material in the presence of machine tool and operational factors.

You do not currently have access to this content.
Don't already have an account? Register

K. Subramanian, 1994. "Classification and Selection of Finishing Processes", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.