Tin Plating

By
Arthur J. Killmeyer
Arthur J. Killmeyer
Revising author
Tin Information Center of North America
Search for other works by this author on:
Published:
1994
Page range:
239 - 241

Abstract

A tin deposit provides sacrificial protection to copper, nickel, and many other nonferrous metals and alloys. Tin also provides good protection to steel. Tin can be deposited from either alkaline or acid electrolytes. This article explains the compositions and operating conditions of these electrolytes.

You do not currently have access to this content.
Don't already have an account? Register

Arthur J. Killmeyer, 1994. "Tin Plating", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal