Skip to Main Content
ASM Handbook

Surface Engineering

Edited by
C.M. Cotell
C.M. Cotell
Search for other works by this author on:
J.A. Sprague
J.A. Sprague
Search for other works by this author on:
F.A. Smidt, Jr.
F.A. Smidt, Jr.
Search for other works by this author on:
ASM International
Volume
5
ISBN electronic:
978-1-62708-170-2
Publication date:
1994
Book Chapter

Indium Plating

By
Allen W. Grobin, Jr.
Allen W. Grobin, Jr.
Grobin Associates, Inc.
Search for other works by this author on:
Published:
1994
Page range:
236 - 238

Abstract

This article focuses on the electrodeposition of indium and its alloys, such as indium-antimony, indium-gallium, and indium-bismuth, in nonaqueous indium plating baths. It also provides information on the stripping of indium plate from plated components and presents an overview of the specifications, standards, and hazards of indium plating.

You do not currently have access to this content.
Don't already have an account? Register

Allen W. Grobin, Jr., 1994. "Indium Plating", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal