Book Chapter

Zinc Plating

By
A. Sato
A. Sato
Revising author
Lea Ronal Inc.
Search for other works by this author on:
Published:
1994
Page range:
227 - 235

Abstract

Commercial zinc plating is accomplished by a number of distinctively different systems: cyanide baths, alkaline noncyanide baths, and acid chloride baths. This article focuses on the composition, advantages, disadvantages, operating parameters, and applications of each of the baths. It provides information on the control of thicknesses of zinc specified for service in various indoor and outdoor atmospheres and on the similarities between cadmium and zinc plating.

You do not currently have access to this content.
Don't already have an account? Register

A. Sato, 1994. "Zinc Plating", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal