Compliant Organic Coatings

By
Thomas E. Kearney
Thomas E. Kearney
Courtaulds Aerospace
Search for other works by this author on:
Published:
1994
Page range:
935 - 939

Abstract

This article discusses coating products available for use in the aerospace industry that are compliant with regulations requiring reductions in emissions from organic solvents. The coating products addressed include primers, topcoats, and chemical milling maskants. It describes their characteristics and limitations compared to conventional noncompliant materials. The article addresses the methods and products commonly used achieve regulatory compliance: waterborne coatings, exempt-solvent-based coatings, high-solids coatings, powder coating, and electro-deposition.

You do not currently have access to this content.
Don't already have an account? Register

Thomas E. Kearney, 1994. "Compliant Organic Coatings", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal