Phosphate Coatings

Published:
1994
Page range:
378 - 404

Abstract

This article focuses on the types, composition, and applications of phosphate coatings and describes the characteristics of phosphate-coated ferrous and nonferrous materials, including steel and aluminum. It addresses five successive process fundamentals: cleaning, rinsing, phosphating, rinsing after phosphating, and chromic acid rinsing. The article describes the techniques for controlling the chemical composition of various phosphating solutions. It discusses the equipment and factors that influence equipment requirements in immersion and spray systems. The article also describes the controlling procedures of coating weight and crystal size. It provides guidelines for choosing phosphate coatings based on application, coating weight requirements, and recommended process parameters. The article concludes with a discussion on safety precautions and the treatment of effluents from phosphating plants.

You do not currently have access to this content.
Don't already have an account? Register

1994. "Phosphate Coatings", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal