Chromium Elimination in Surface Engineering

By
Barry Meyers
Barry Meyers
The MITRE Corporation
Search for other works by this author on:
Stephen Lynn
Stephen Lynn
The MITRE Corporation
Search for other works by this author on:
Elwin Jang
Elwin Jang
United States Air Force, Sacramento Air Logistics Center
Search for other works by this author on:
Published:
1994
Page range:
925 - 929

Abstract

This article focuses on alternatives to chromium in both hard chromium plating and chromate conversion coating. These include electroless nickel plating, nickel-tungsten composite electroplating, spray coating applications, and cobalt/molybdenum-base conversion coating. The article discusses the material and process substitutions that can be used to eliminate the use or emissions of chromium in industrial processes. It describes the physical characteristics of each coating, economics, environmental impacts, advantages, and disadvantages of alternative processes.

You do not currently have access to this content.
Don't already have an account? Register

Barry Meyers, Stephen Lynn, Elwin Jang, 1994. "Chromium Elimination in Surface Engineering", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal