By
Sue Troup-Packman
Sue Troup-Packman
Hughes Research Laboratories
Search for other works by this author on:
Published:
1994
Page range:
213 - 214

Abstract

Iron has been electroplated from a variety of electrolytes, whose bath parameters result in coatings that have widely divergent characteristics according to the specific characteristics desired in the finished product. This article provides an overview of the process description and processing equipment and discusses the properties, advantages, limitations, and principal applications of iron plating. It also describes the environmental, health, and safety considerations of iron plating.

You do not currently have access to this content.
Don't already have an account? Register

Sue Troup-Packman, 1994. "Iron Plating", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.