Acid Cleaning

By
Kenneth J. Hacias
Kenneth J. Hacias
Revising author
Parker + Amchem, Henkel Corporation
Search for other works by this author on:
Published:
1994
Page range:
48 - 54

Abstract

This article focuses on the mineral and organic acid cleaning of iron and steel. It begins with a discussion on the application methods, process selection criteria, solution composition, equipment used, and control of process variables in mineral acid cleaning. The article then describes the advantages and disadvantages of organic acid cleaning. Applications, including boiler cleaning, stainless steel cleaning, and removal of iron- and copper-bearing deposits, are discussed. The article concludes with an overview of acid cleaning of nonferrous alloys.

You do not currently have access to this content.
Don't already have an account? Register

Kenneth J. Hacias, 1994. "Acid Cleaning", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal