Molten Salt Bath Cleaning

By
James C. Malloy
James C. Malloy
Kolene Corporation
Search for other works by this author on:
Published:
1994
Page range:
39 - 42

Abstract

Molten salt baths are anhydrous, fused chemical baths used at elevated temperatures for a variety of industrial cleaning applications. This article discusses their applications in paint stripping, polymer removal, casting cleaning, glass removal, and plasma/flame spray removal. It provides an overview of the basic design and safety considerations of the salt bath equipment and describes the environmental impact of molten salt bath cleaning.

You do not currently have access to this content.
Don't already have an account? Register

James C. Malloy, 1994. "Molten Salt Bath Cleaning", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal