Surface Preparation for Continuously Applied Coatings

By
Curtiss Dunbar
Curtiss Dunbar
LTV Steel Company
Search for other works by this author on:
Published:
1994
Page range:
335 - 338

Abstract

This article focuses on the various techniques for removing contaminants in the surface preparation of steel for hot-dip coatings: wet cleaning methods, including alkaline cleaning, electrolytic cleaning, chemical pickling, and electrolytic pickling; flame cleaning and furnace-atmosphere techniques, such as Sendzimir oxidation/reduction method; other specialized methods, namely, fluxes, mechanical cleaning, and ultrasonic methods; or a combination of these.

You do not currently have access to this content.
Don't already have an account? Register

Curtiss Dunbar, 1994. "Surface Preparation for Continuously Applied Coatings", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal