Plasma Surface Engineering of Plastics

By
Om S. Kolluri
Om S. Kolluri
AIRCO Coating Technology
Search for other works by this author on:
Published:
1994
Page range:
892 - 899

Abstract

This article provides an overview of plasma surface treatments for plastics. It covers the equipment and methods used in plasma processing, providing detailed explanations of the plasma discharge reactions and how they affect surface state and topography. It also provides information on contamination removal, plasma surface modification, plasma-induced grafting, and plasma film deposition.

You do not currently have access to this content.
Don't already have an account? Register

Om S. Kolluri, 1994. "Plasma Surface Engineering of Plastics", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.