Multiple-Layer Alloy Plating

By
Daniel T. Schwartz
Daniel T. Schwartz
University of Washington
Search for other works by this author on:
Published:
1994
Page range:
274 - 276

Abstract

Multiple-layer alloy electrodeposition involves the formation of an inhomogeneous alloy consisting of lamellae of different composition. This article reviews the process description, engineering parameters, characterization, and applications of multiple-layer alloys. Pulsed-current plating and pulsed-potential plating are also discussed.

You do not currently have access to this content.
Don't already have an account? Register

Daniel T. Schwartz, 1994. "Multiple-Layer Alloy Plating", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal