Skip to Main Content
ASM Handbook

Surface Engineering

Edited by
C.M. Cotell
C.M. Cotell
Search for other works by this author on:
J.A. Sprague
J.A. Sprague
Search for other works by this author on:
F.A. Smidt, Jr.
F.A. Smidt, Jr.
Search for other works by this author on:
ASM International
Volume
5
ISBN electronic:
978-1-62708-170-2
Publication date:
1994
Book Chapter

Chromium Alloy Plating

By
Eric W. Brooman
Eric W. Brooman
Concurrent Technologies Corporation
Search for other works by this author on:
Published:
1994
Page range:
270 - 273

Abstract

Chromium alloys yield alloy coatings with properties that range from completely satisfactory to marginally acceptable, depending on the end use. This article provides a detailed description of plating solutions and deposition conditions and rates of chromium-iron, chromium-nickel, and chromium-iron-nickel alloys.

You do not currently have access to this content.
Don't already have an account? Register

Eric W. Brooman, 1994. "Chromium Alloy Plating", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal