Tin Alloy Plating

By
Reginald K. Asher, Sr.
Reginald K. Asher, Sr.
Motorola Semiconductor Product Sector
Search for other works by this author on:
Published:
1994
Page range:
258 - 263

Abstract

Electrodeposition of tin alloys is used to protect steel against corrosion or wear, to impart resistance to etching, and to facilitate soldering. This article focuses on the compositions, operating conditions, advantages, and limitations of methane sulfonic acid plating solutions and fluoborate plating solutions for tin-lead. It briefly describes the solution compositions and operating conditions of tin-bismuth, tin-nickel, and tin-zinc.

You do not currently have access to this content.
Don't already have an account? Register

Reginald K. Asher, Sr., 1994. "Tin Alloy Plating", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal