Surface Engineering of Titanium and Titanium Alloys

By
A. Bloyce
A. Bloyce
University of Birmingham
,
U.K.
Search for other works by this author on:
P.H. Morton
P.H. Morton
University of Birmingham
,
U.K.
Search for other works by this author on:
T. Bell
T. Bell
University of Birmingham
,
U.K.
Search for other works by this author on:
Published:
1994
Page range:
835 - 851

Abstract

This article reviews cleaning and finishing operations that have proven to be effective on titanium, its alloys, and semi-fabricated titanium products. It explains how to remove scale, tarnish films, grease, and other soils and how to achieve required finishes and/or improve wear and oxidation resistance through the use of polishing, buffing, and wire brushing operations. The article also covers a wide range of surface modification and coating processes, including ion implantation, diffusion, chemical and physical vapor deposition, plating, anodizing, and chemical conversion coatings as well as sprayed and sol-gel coatings and laser and electron-beam treatments.

You do not currently have access to this content.
Don't already have an account? Register

A. Bloyce, P.H. Morton, T. Bell, 1994. "Surface Engineering of Titanium and Titanium Alloys", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.