Skip to Main Content
ASM Handbook

Surface Engineering

Edited by
C.M. Cotell
C.M. Cotell
Search for other works by this author on:
J.A. Sprague
J.A. Sprague
Search for other works by this author on:
F.A. Smidt, Jr.
F.A. Smidt, Jr.
Search for other works by this author on:
ASM International
Volume
5
ISBN electronic:
978-1-62708-170-2
Publication date:
1994
Book Chapter

Anodizing

By
Milton F. Stevenson, Jr.
Milton F. Stevenson, Jr.
Revising author
Anoplate Corporation
Search for other works by this author on:
Published:
1994
Page range:
482 - 493

Abstract

Anodizing refers to conversion coating of the surface of aluminum and its alloys to porous aluminum oxide. This article provides the reasons for performing anodizing and discusses the three principal types of anodizing processes, namely, chromic acid process, sulfuric acid process, and hard anodic process. It describes the limitations imposed by variables, such as alloy composition, surface finish, prior processing, temper or heat treatment, and the use of inserts, on the anodizing processes. The article explains the causes and means adopted for correcting several specific problems in anodizing aluminum. It also discusses the process control techniques and equipment used for anodizing. The article reviews the sealing processes for anodic coatings and the method for coloring the coatings. It concludes with a discussion on the effects of anodic coatings on the surface and mechanical properties of aluminum and its alloys.

You do not currently have access to this content.
Don't already have an account? Register

Milton F. Stevenson, Jr., 1994. "Anodizing", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal