Skip to Main Content
ASM Handbook

Surface Engineering

Edited by
C.M. Cotell
C.M. Cotell
Search for other works by this author on:
J.A. Sprague
J.A. Sprague
Search for other works by this author on:
F.A. Smidt, Jr.
F.A. Smidt, Jr.
Search for other works by this author on:
ASM International
Volume
5
ISBN electronic:
978-1-62708-170-2
Publication date:
1994
Book Chapter

Arc Deposition

By
David M. Sanders
David M. Sanders
Lawrence Livermore National Laboratory
Search for other works by this author on:
Joseph W. Glaser
Joseph W. Glaser
Lawrence Livermore National Laboratory
Search for other works by this author on:
Steven Falabella
Steven Falabella
Lawrence Livermore National Laboratory
Search for other works by this author on:
Published:
1994
Page range:
602 - 604

Abstract

This article describes the characteristics of continuous cathodic arc sources and filtering process for removing macroparticles from a cathodic arc. It provides information on the types of arc sources and the properties of deposited materials. The advantages, limitations, and applications of arc deposition are also discussed.

You do not currently have access to this content.
Don't already have an account? Register

David M. Sanders, Joseph W. Glaser, Steven Falabella, 1994. "Arc Deposition", Surface Engineering, C.M. Cotell, J.A. Sprague, F.A. Smidt, Jr.