Hardness and Hardenability of Steels[1]

Published:
2013
Page range:
26 - 59
Publication history
July 08, 2013

Abstract

Hardenability refers to the ability of steel to obtain satisfactory hardening to some desired depth when cooled under prescribed conditions. It is governed almost entirely by the chemical composition (carbon and alloy content) at the austenitizing temperature and the austenite grain size at the moment of quenching. This article describes the Jominy end-quench test, the Grossman method, and the air hardenability test to evaluate hardenability. It also reviews the factors that influence steel hardenability and selection.

You do not currently have access to this content.
Don't already have an account? Register

2013. "Hardness and Hardenability of Steels", Steel Heat Treating Fundamentals and Processes, Jon L. Dossett, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal