Intensive Quenching of Steel Parts

By
Michael A. Aronov
Michael A. Aronov
IQ Technologies, Inc.
Search for other works by this author on:
Nikolai I. Kobasko
Nikolai I. Kobasko
IQ Technologies, Inc.
Search for other works by this author on:
Joseph A. Powell
Joseph A. Powell
IQ Technologies, Inc.
Search for other works by this author on:
George E. Totten
George E. Totten
Portland State University
Search for other works by this author on:
Published:
2013
Page range:
198 - 212
Publication history
July 03, 2013

Abstract

Intensive quenching (IQ) is an alternative method of hardening steel parts, providing extremely high cooling rates within the martensite-phase formation temperature range. This article begins with the description on the general correlation between steel mechanical properties and cooling rate during IQ. It presents a review of batch intensive quenching (IQ-2) methods and single-part intensive quenching (IQ-3) methods as well as practical applications of these methods. The article provides useful information on the effect of heat flow on cooling in these methods, and discusses the improvements achieved in part microstructure, mechanical properties, and stress conditions of steel, after intensive quenching. It also describes the reasons for part distortion in IQ, and reviews the types of quench systems used in IQ-2 and IQ-3 processes.

You do not currently have access to this content.
Don't already have an account? Register

Michael A. Aronov, Nikolai I. Kobasko, Joseph A. Powell, George E. Totten, 2013. "Intensive Quenching of Steel Parts", Steel Heat Treating Fundamentals and Processes, Jon L. Dossett, George E. Totten