Evaluation of Carbon Control in Carburized Parts

By
Gary D. Keil
Gary D. Keil
Caterpillar Inc.
Search for other works by this author on:
Olga K. Rowan
Olga K. Rowan
Caterpillar Inc.
Search for other works by this author on:
Published:
2013
Page range:
522 - 527
Publication history
July 16, 2013

Abstract

This article presents the different hardness test methods used to measure the effectiveness of surface carbon control in carburized parts of steel. Common test methods include Rockwell hardness measurements, superficial Rockwell 15N testing, and microhardness testing. The article provides information on the microscopic method used to detect smaller variations in carbon content, and reviews consecutive cuts analysis and spectrographic analysis that are used to accurately evaluate the carbon concentration profile of carburized parts. It describes procedures of and precautions to be undertaken during shim stock analysis, which is used to measure the atmosphere carbon potential. The article includes a discussion on the electromagnetic nondestructive tests that are used to evaluate the case depth of case-hardened parts.

You do not currently have access to this content.
Don't already have an account? Register

Gary D. Keil, Olga K. Rowan, 2013. "Evaluation of Carbon Control in Carburized Parts", Steel Heat Treating Fundamentals and Processes, Jon L. Dossett, George E. Totten

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal