H Steels and Steel Selection for Hardenability[1]

Published:
1990
Page range:
1 - 19
Publication history
March 30, 2017

Abstract

Hardenability is an expression of the propensity of steel to harden when quenched at the austenitizing temperature. It is defined in terms of the depth and distribution of alloying elements present in the steel. This article describes the selection process for steel with an emphasis on hardenability. It explains the significance of H-steels, and how they are guaranteed to meet established hardenability limits for specific temperatures and chemical compositions. The article compares hardenability curves for six series of steel and includes several charts showing composition and H-band limits for various alloy grades.

You do not currently have access to this content.
Don't already have an account? Register

1990. "H Steels and Steel Selection for Hardenability", Properties and Selection: Irons, Steels, and High-Performance Alloys, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal