Abstract

Malleable iron possesses considerable ductility and toughness because of its combination of nodular graphite and a low-carbon metallic matrix. The desired formation of temper carbon in malleable irons has two basic requirements. First, graphite should not form during the solidification of the white cast iron, and second, graphite must also be readily formed during the annealing heat treatment. These two metallurgical requirements influence the useful compositions of malleable irons and the melting, solidification, and annealing procedures. There are two basic types of malleable iron: blackheart and whiteheart. This article considers only the blackheart type and describes the metallurgical factors of malleable iron. It discusses the mechanical properties of pearlitic and martensitic malleable irons. The article provides additional information on the properties and heat treatment of ferritic, pearlitic, and martensitic malleable irons. The article lists some of the typical applications of malleable iron castings.

You do not currently have access to this content.
Don't already have an account? Register

1990. "Malleable Iron", Properties and Selection: Irons, Steels, and High-Performance Alloys, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal