Skip to Main Content
ASM Handbook

Properties and Selection: Irons, Steels, and High-Performance Alloys

By
ASM Handbook Committee
ASM Handbook Committee
Search for other works by this author on:
ASM International
Volume
1
ISBN electronic:
978-1-62708-161-0
Publication date:
1990
Book Chapter

Cast Stainless Steels

By
Malcolm Blair
Malcolm Blair
Revising author
Steel Founders' Society of America
Search for other works by this author on:
Published:
1990
Page range:
908 - 929

Abstract

This article reviews the properties of cast steels that are specified for liquid corrosion service at temperatures above and below 650 deg C. Stainless steel castings are usually classified based on their resistance to corrosion and heat and generally fall into one category or the other. The article describes alternate methods for classifying cast stainless steels, one is based on grade designations, the other on microstructural analysis. It also addresses heat treatment, pointing out its similarities with the thermal processing of wrought materials, and establishes the importance of mechanical properties in material selection. The article presents information on the selection process and provides a detailed list of heat-resistant cast steels and alloys. It also includes key manufacturing characteristics to aid in foundry and welding-related decisions.

You do not currently have access to this content.
Don't already have an account? Register

Malcolm Blair, 1990. "Cast Stainless Steels", Properties and Selection: Irons, Steels, and High-Performance Alloys, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal