Skip to Main Content
ASM Handbook

Properties and Selection: Nonferrous Alloys and Special-Purpose Materials

By
ASM Handbook Committee
ASM Handbook Committee
Search for other works by this author on:
ASM International
Volume
2
ISBN electronic:
978-1-62708-162-7
Publication date:
1990
Book Chapter

Preparation and Characterization of Pure Metals

By
G.T. Murray
G.T. Murray
Materials Engineering Department, California Polytechnic State University
Search for other works by this author on:
;
T.A. Lograsso
T.A. Lograsso
Ames Laboratory, Iowa State University
Search for other works by this author on:
Published:
1990
Page range:
1093 - 1097

Abstract

The electronic microcircuit industry has placed severe demands on metal suppliers to provide metals of the highest reproducible purity attainable as a result of the constant quest for the true values of physical and chemical properties of metals. This Article describes the commonly used methods for ultrapurification of metals produced by electrolytic processes, including fractional crystallization, zone refining, vacuum melting, distillation, chemical vapor deposition, and solid state refining techniques. In addition, it describes the trace element analysis and resistance-ratio test methods used to characterize purity. Tables list the values for resistance ratios of zone-refined metals and their corresponding chemical compositions, and provide an example of the detection of impurities to concentrations in the parts per billion range, utilizing a combination of the glow discharge mass spectroscopy method and Leco combustion methods.

You do not currently have access to this content.
Don't already have an account? Register

G.T. Murray, T.A. Lograsso, 1990. "Preparation and Characterization of Pure Metals", Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook Committee

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal