Skip to Main Content
ASM Handbook

Properties and Selection: Nonferrous Alloys and Special-Purpose Materials

By
ASM Handbook Committee
ASM Handbook Committee
Search for other works by this author on:
ASM International
Volume
2
ISBN electronic:
978-1-62708-162-7
Publication date:
1990
Book Chapter

Superabrasives and Ultrahard Tool Materials

By
T.J. Clark
T.J. Clark
G.E. Superabrasives
Search for other works by this author on:
;
R.C. DeVries
R.C. DeVries
G.E. Corporate Research and Development Center

Retired

Search for other works by this author on:
Published:
1990
Page range:
1008 - 1018

Abstract

The principal superhard materials are found as phases in the boron-carbon-nitrogen-silicon family of elements. Of these, the superhard materials of commercial interest include silicon nitride (Si3N4), silicon carbide (SiC), boron carbide (B4C), diamond, and cubic boron nitride (CBN). This Article describes the synthesis of diamond and cubic boron nitride (CBN) for transforming a crystal structure from a soft hexagonal form to a hard cubic form. Polycrystalline diamond (PCD) or polycrystalline CBN (PCBN) are produced by sintering (or binding) many individual crystals of diamond or CBN together to produce a larger polycrystalline mass. The Article also provides useful information on the physical properties of diamond, CBN, and sintered polycrystalline diamond. Further, the Article describes superabrasive grains that are commercially available in a range of sizes, shapes, and qualities. Diamond or CBN grains can be used as loose abrasives, as bonded abrasives in grinding wheels and hones, and as bonded abrasives in single-point applications such as turning tools, dressers, and scribes. Finally, the Article provides a short note on the applications of ultrahard cutting tool materials of sintered PCD or PCBN.

You do not currently have access to this content.
Don't already have an account? Register

T.J. Clark, R.C. DeVries, 1990. "Superabrasives and Ultrahard Tool Materials", Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook Committee

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal