Electrical Resistance Alloys

By
Robert A. Watson
Robert A. Watson
Revising author
The Kanthal Corporation
Search for other works by this author on:
Bo Jönsson
Bo Jönsson
Revising author
Kanthal AB
Search for other works by this author on:
George A. Fielding
George A. Fielding
Revising author
Harrison Alloys, Inc.
Search for other works by this author on:
Donald V. Cunningham
Donald V. Cunningham
Revising author
Emerson Electric, Wiegand Division
Search for other works by this author on:
C. Dean Starr
C. Dean Starr
Revising author
C. Dean Starr, Inc.
Search for other works by this author on:
Published:
1990
Page range:
822 - 839

Abstract

Electrical resistance alloys include those types used in instruments, control equipments, heating elements, and devices that convert heat generated to mechanical energy. This Article discusses the basic classification of electrical resistance alloys (resistance alloys, heating alloys, and thermostat metals), their subtypes, properties, service life, and operating temperatures. It describes the designing and fabrication of open resistance and sheathed heaters. The Article contains a collection of tables and graphs that provide information on the mechanical properties, chemical composition, temperature coefficient of resistance, furnace operating temperatures, length and spacing of loops, ribbon size, and electrical capacity of heating elements.

You do not currently have access to this content.
Don't already have an account? Register

Robert A. Watson, Bo Jönsson, George A. Fielding, Donald V. Cunningham, C. Dean Starr, 1990. "Electrical Resistance Alloys", Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal