Skip to Main Content
ASM Handbook

Properties and Selection: Nonferrous Alloys and Special-Purpose Materials

By
ASM Handbook Committee
ASM Handbook Committee
Search for other works by this author on:
ASM International
Volume
2
ISBN electronic:
978-1-62708-162-7
Publication date:
1990
Book Chapter

Metallic Glasses

By
W.L. Johnson
W.L. Johnson
Keck Laboratory of Engineering, California Institute of Technology
Search for other works by this author on:
Published:
1990
Page range:
804 - 821

Abstract

Metallic glasses can be prepared by solidification of liquid alloys at cooling rates sufficient to suppress the nucleation and growth of competing crystalline phases. This Article presents a historical survey of the study of metallic glasses and other amorphous metals and alloys. This includes a discussion of synthesis and processing methods, structure and morphology, and a description of the electronic, magnetic, thermodynamic, chemical, and mechanical properties of metallic glasses. In addition, the Article describes the development of metallic glasses as materials for technical applications.

You do not currently have access to this content.
Don't already have an account? Register

W.L. Johnson, 1990. "Metallic Glasses", Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal