Permanent Magnet Materials

By
J.W. Fiepke
J.W. Fiepke
Revising author
Crucible Magnetics, a Division of Crucible Materials Corporation
Search for other works by this author on:
Published:
1990
Page range:
782 - 803

Abstract

This Article discusses the chief magnetic characteristics of permanent magnet materials. It provides a detailed description on nominal compositions; principal magnet designations; magnetic, physical, and mechanical properties; selection criteria; and applications of the permanent magnet materials, which include magnet steels, magnet alloys, alnico alloys, platinum-cobalt alloys, cobalt and rare-earth alloys, hard ferrites, iron-chromium-cobalt alloys, and neodymium-iron-boron alloys.

You do not currently have access to this content.
Don't already have an account? Register

J.W. Fiepke, 1990. "Permanent Magnet Materials", Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal