Skip to Main Content
ASM Handbook

Properties and Selection: Nonferrous Alloys and Special-Purpose Materials

By
ASM Handbook Committee
ASM Handbook Committee
Search for other works by this author on:
ASM International
Volume
2
ISBN electronic:
978-1-62708-162-7
Publication date:
1990
Book Chapter

Properties of Wrought Coppers and Copper Alloys

By
Peter Robinson
Peter Robinson
Revising author
Olin Corporation
Search for other works by this author on:
Published:
1990
Page range:
265 - 345

Abstract

This Article is a compilation of the property data for standard grades of wrought copper and copper alloys. Data are provided for mechanical, physical, thermal, electrical, optical, and magnetic properties. The list for each alloy includes its commercial names, chemical composition, relevant specifications and standards, fabrication characteristics, mass characteristics, and applications.

You do not currently have access to this content.
Don't already have an account? Register

Peter Robinson, 1990. "Properties of Wrought Coppers and Copper Alloys", Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal