This Article briefly reviews the subject of copper-base powder-metallurgy (P/M) products in terms of powder production methods (atomization, oxide reduction, electrolysis, and hydrometallurgy) and the product properties/consolidation practices of the major applications. Of the four major methods for making copper and copper alloy powders, atomization and oxide reduction are presently practiced on a large scale in North America. The Article provides information on the mechanism, production, properties, composition and applications of different types of copper-base P/M products, including self-lubricating sintered bearings, structural parts, oxide-dispersion-strengthened copper, sintered metal friction materials, and porous filters.
Sign in
ASM members
Member Sign InErhard Klar, David F. Berry, 1990. "Copper Powder Metallurgy Products", Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook Committee
Download citation file:
×
Advertisement
Mager
Mager Scientific is your exclusive source for Qness hardness testing equipment in the United States.