Properties and Selection: Nonferrous Alloys and Special-Purpose Materials

By
ASM Handbook Committee
ASM Handbook Committee
Search for other works by this author on:
ASM International
Volume
2
ISBN electronic:
978-1-62708-162-7
Publication date:
1990
Book Chapter

Properties of Precious Metals

Published:
1990
Page range:
699 - 719

Abstract

This Article discusses the chemical composition, fabrication characteristics, applications, mechanical properties, mass characteristics, thermal properties, electrical properties, optical properties, and chemical properties of precious metals, namely, silver, gold, platinum, and palladium and their corresponding alloys.

You do not currently have access to this content.
Don't already have an account? Register

1990. "Properties of Precious Metals", Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal