Metal-Matrix Composites

By
John V. Foltz
John V. Foltz
Metallic Materials Branch, Naval Surface Warfare Center, White Oak Laboratory
Search for other works by this author on:
Charles M. Blackmon
Charles M. Blackmon
Applied Materials Technology Branch, Naval Surface Warfare Center, Dahlgren Laboratory
Search for other works by this author on:
Published:
1990
Page range:
903 - 912

Abstract

Metal-matrix composites (MMCs) are a class of materials with potential for a wide variety of structural and thermal management applications. They are nonflammable, do not outgas in a vacuum, and suffer minimal attack by organic fluids, such as fuels and solvents. This Article presents an overview of the status of MMCs, and provides information on physical and mechanical properties, processing methods, distinctive features, and various types of continuously and discontinuously reinforced aluminum, magnesium, titanium, copper, superalloy, and intermetallic-matrix composites. It further discusses the property prediction and processing methods for MMCs.

You do not currently have access to this content.
Don't already have an account? Register

John V. Foltz, Charles M. Blackmon, 1990. "Metal-Matrix Composites", Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook Committee

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal