Book Chapter

Specific Metals and Alloys

Published:
1990

Abstract

Aluminum, the second most plentiful metallic element, is an economic competitor in various applications owing to its appearance, light weight, fabricability, physical properties, mechanical properties, and corrosion resistance. This Article discusses the primary and secondary production of aluminum and classification system for cast and wrought aluminum alloys. It talks about various manufactured forms of aluminum and its alloys, which are classified into standardized products such as sheet, plate, foil, rod, bar, wire, tube, pipe, and structural forms, and engineered products such as extruded shapes, forgings, impacts, castings, stampings, powder metallurgy parts, machined parts, and metal-matrix composites. The Article also reviews important fabrication characteristics in the machining, forming, forging, and joining of aluminum alloys. It concludes with a description of the major industrial applications of aluminum, including building and construction, transportation, consumer durables, electrical, machinery and equipment, containers and packaging, and other applications.

You do not currently have access to this content.
Don't already have an account? Register

1990. "Specific Metals and Alloys", Properties and Selection: Nonferrous Alloys and Special-Purpose Materials, ASM Handbook Committee