Skip to Main Content
ASM Handbook

Protective Organic Coatings

Edited by
Kenneth B. Tator
Kenneth B. Tator
KTA-Tator, Inc.
Search for other works by this author on:
ASM International
Volume
5B
ISBN electronic:
978-1-62708-172-6
Publication date:
2015
Book Chapter

Pipeline Industry Coatings

By
E. Bud Senkowski
E. Bud Senkowski
KTA-Tator, Inc.
Search for other works by this author on:
Published:
2015
Page range:
327 - 339
Publication history
December 26, 2014

Abstract

This article describes the coating materials, surface-preparation requirements, and application techniques used to protect underground pipelines. It provides a valuable insight into the types of polymer-based coatings that are both cost-effective and widely accepted in the pipeline industry.

You do not currently have access to this content.
Don't already have an account? Register

E. Bud Senkowski, 2015. "Pipeline Industry Coatings", Protective Organic Coatings, Kenneth B. Tator

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal