Protective Organic Coatings
Protective Coatings for Corrosion Control in Municipal Wastewater Systems
Abstract
This article provides information on the municipal wastewater system components such as piping, pump stations, headworks, clarifiers, aeration structures, digesters, biosolids dewatering equipment, and sludge stabilization. It explains the major corrosion damage mechanisms to which those component parts of the system are exposed. It presents useful guidelines for selecting and using protective coatings in municipal sewerage collection systems and water reclamation facilities in wastewater treatment plants. The article includes annotated flow diagrams of a wastewater collection system, wastewater treatment plants, and spreadsheets listing the most widely used generic coating systems by structure and substrate material. It concludes with a section on quality watchouts when selecting or using protective coatings in municipal wastewater systems.
Sign in
ASM members
Member Sign InR.A. Nixon, 2015. "Protective Coatings for Corrosion Control in Municipal Wastewater Systems", Protective Organic Coatings, Kenneth B. Tator
Download citation file:
×
Advertisement
Mager
Mager Scientific is your exclusive source for Qness hardness testing equipment in the United States.