Skip to Main Content
ASM Handbook

Protective Organic Coatings

Edited by
Kenneth B. Tator
Kenneth B. Tator
KTA-Tator, Inc.
Search for other works by this author on:
ASM International
Volume
5B
ISBN electronic:
978-1-62708-172-6
Publication date:
2015
Book Chapter

Powder Coatings—Other Industries

By
Denis Grimshaw
Denis Grimshaw
Jotun Powder Coatings
Search for other works by this author on:
Published:
2015
Page range:
168 - 176
Publication history
December 26, 2014

Abstract

Powder coatings are widely used by manufacturers as a finish of choice to enhance the appearance and performance of their products. This article begins with a discussion on advantages and disadvantages of powder coatings. It describes the selection of coating-types and uses of powder coatings in appliance industries, furniture industries, computer industries, fixture industries, architectural industries, automotive industries, agriculture and construction equipment industries, recreational equipment industries, and general industries. Powder coating formulations consist of binder systems, pigments, extenders, and additives. The basic process flow for the manufacture of powder coatings consists of premix, extrusion, grinding, and packing. The article also provides information on application of powder coatings, including pretreatment, deposition, and curing as well as on troubleshooting, trends and challenges for the powder coatings.

You do not currently have access to this content.
Don't already have an account? Register

Denis Grimshaw, 2015. "Powder Coatings—Other Industries", Protective Organic Coatings, Kenneth B. Tator

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal