Coating Failure Analysis

By
Rick Huntley
Rick Huntley
KTA-Tator, Inc.
Search for other works by this author on:
Published:
2015
Page range:
474 - 482
Publication history
December 26, 2014

Abstract

This article discusses the standard conduct of coating failure investigation. As each failure is different, a specific coating failure may require increased emphasis on a given step, or additional work and/or steps may be required. This article covers the following topics: obtaining and analyzing background information, preliminary determination of site conditions, inspection equipment requirements, coating failure site investigation, sampling techniques, sample chain of custody, coordination with the coatings laboratory, report preparation, and sample retention.

You do not currently have access to this content.
Don't already have an account? Register

Rick Huntley, 2015. "Coating Failure Analysis", Protective Organic Coatings, Kenneth B. Tator